Material: 3mm ABS (Velleman from reprapuniverse.com)
Hotend: 245°C 1st layer, then 240°C
Heatbed: 115°C 1st layer, then 110°C
Heatbed adhesion: 3 layers of Fructis Bamboo Extract Hairspray, extra hold nr 6
Layer height: 0,2mm
Nozzle: 0,4mm
Gcode generated with Slic3r
Object printed with Pronterface
Issues
- the 10mm bridge is not that clean, the 5mm bridge is perfect though
- object is warping after some layers, need to find out why (more adhesion needed?, heatbed temp too high?, etc?)
- corners for short edges are more rounded off than corners for long edges (top 5 mm)
Good stuff
- Extrusion calibration is near perfect
- X, Y & Z-axis calibration is near perfect (calipers confirm!)
Maybe try PLA next?